题名: Air-Oxidation Behavior of a [(Co50Cr15Mo14C15B6)97.5Er2.5]93Fe7Bulk-Metallic Glass at 873 K to 973 K (600 C to 700o C)
作者: WU KAI;YUAN-HAO WU;WEI SHEN CHEN;RONG-TAN HUANG;HAOLING JIA;PETER K. LIAW;TAO ZHANG
開物
贡献者: NTOU:Institute of Materials Engineering
日期: 2012-08-01
上传时间: 2013-10-07T02:02:30Z
出版者: METALLURGICAL AND MATERIALS TRANSACTIONS A
摘要: The oxidation behavior of a [(Co50Cr15Mo14C15B6)97.5Er2.5]93Fe7 bulk-metallic glass (Co7-BMG) was studied over the temperature range of 873 K to 973 K (600 °C to 700 °C) in dry air. The oxidation kinetics of the Co7-BMG generally followed the parabolic-rate law, as its oxidation rates increased with temperature. The scaling rate of the Co7-BMG was significantly lower than that of pure Co, which indicates a better oxidation resistance for the amorphous alloy. The scales formed on the Co7-BMG consisted mostly of CoMoO4 and Co3O4, as well as minor amounts of CoO, Cr2O3, and uncorroded Co3B. The formation of CoMoO4 and Cr2O3 is responsible for the lower oxidation rates of the glassy alloy with respect to those of pure Co. In addition, the presence of Co3B further indicated that the crystallization of the amorphous substrate during the oxidation was taken place.
關聯: 43(8), pp.2721-2728
URI: http://ntour.ntou.edu.tw/handle/987654321/34166
显示于类别:[材料工程研究所] 期刊論文

文件中的档案:

档案 描述 大小格式浏览次数
index.html0KbHTML181检视/开启


在NTOUR中所有的数据项都受到原著作权保护.

 


著作權政策宣告: 本網站之內容為國立臺灣海洋大學所收錄之機構典藏,無償提供學術研究與公眾教育等公益性使用,請合理使用本網站之內容,以尊重著作權人之權益。
網站維護: 海大圖資處 圖書系統組
DSpace Software Copyright © 2002-2004  MIT &  Hewlett-Packard  /   Enhanced by   NTU Library IR team Copyright ©   - 回馈