题名: The oxidation behavior of Cu–Zr–Ti–base bulk metallic glasses in air at 350–500 °C
作者: H. H. Hsieh;W. Kai;W. L. Jang;R. T. Huang;P. Y. Lee;W. H. Wang
贡献者: NTOU:Institute of Materials Engineering
國立臺灣海洋大學:材料工程研究所
关键词: Bulk metallic alloys;CuO;Cu2O;ZrO2;ZrTiO4;Zr5Ti7O24
日期: 2007-04-01
上传时间: 2011-10-20T08:06:54Z
出版者: Oxidation of Metals
摘要: Abstract:The oxidation behavior of two Cu-base bulk metallic glasses (BMGs), having compositions Cu–30Zr–10Ti and Cu–20Zr–10Ti–10Hf (in at.%), was studied over the temperature range of 350–500 °C in dry air. In general, the oxidation kinetics of both BMGs followed the parabolic rate law, with the oxidation rates increasing with increasing temperature. The addition of Hf slightly reduced the oxidation rates at 350–400 °C, while the opposite results observed at higher temperatures. It was found that the oxidation rates of both BMGs were significantly higher than those of polycrystalline pure-Cu. The scales formed on both BMG alloys were strongly composition dependent, consisting of mostly CuO/Cu2O and minor amounts of cubic-ZrO2 and ZrTiO4 for the ternary BMG, and of CuO, cubic-ZrO2, and Zr5Ti7O24 for the quaternary BMG. The formation of ternary oxides (ZrTiO4 and Zr5Ti7O24) was inferred to be responsible for the fast oxidation rates of the BMGs.
關聯: 67(3-4), pp.179–192
URI: http://ntour.ntou.edu.tw/handle/987654321/23638
显示于类别:[材料工程研究所] 期刊論文

文件中的档案:

档案 描述 大小格式浏览次数
index.html0KbHTML335检视/开启


在NTOUR中所有的数据项都受到原著作权保护.

 


著作權政策宣告: 本網站之內容為國立臺灣海洋大學所收錄之機構典藏,無償提供學術研究與公眾教育等公益性使用,請合理使用本網站之內容,以尊重著作權人之權益。
網站維護: 海大圖資處 圖書系統組
DSpace Software Copyright © 2002-2004  MIT &  Hewlett-Packard  /   Enhanced by   NTU Library IR team Copyright ©   - 回馈